For the same grain size and hardness in the unembrittled conditions, martensite has lower yield strength higher Charpy fracture energy and lower FATT due to finer mean carbide size.
在同样晶粒度和硬度,不添加杂质的条件下,马氏体有较低的屈服强度、较高的冲击断裂功以及较低的塑脆转变温度,这些都由于较细的平均碳化物尺寸引起。
The wide range of investigations shown shut lower yield strength, coarse grain size and metallurgical flaws were the basic causes for the earlier failure of superalloy for turbine disk.
广泛的研究表明,屈服强度低、粗晶粒尺寸、冶金缺陷的存在是造成涡轮盘用高温合金早期失效的主要原因。
By pressing at very much higher temperatures lower pressures are required as the yield strength of the material is lower.
由于很高温度下材料的屈服强度较低,因此只需较低压力就能挤压。