• 不透返修尽量采用间歇和分段气减少热量输入,彻底清除渗碳层,露出金属光泽后方可焊接。

    For the repair of stainless steel, to reduce heat energy and clean completely, gouging should in discontinuous way.

    youdao

  • 通过13 -5型马氏体不锈焊接接头进行等离子清根及弧气清根比较证明等离子弧清根焊透焊缝实施背面清根是可行的。

    By comparing backgouging of plasma arc with carbon arc to the welded joint of 13-5 martensitic stainless steel, the backgouging of plasma arc is proved feasible for the full penetration weld.

    youdao

  • 通过13 -5型马氏体不锈焊接接头进行等离子清根及弧气清根比较证明等离子弧清根焊透焊缝实施背面清根是可行的。

    By comparing backgouging of plasma arc with carbon arc to the welded joint of 13-5 martensitic stainless steel, the backgouging of plasma arc is proved feasible for the full penetration weld.