• 不透钢的返修,应尽量采用间歇和分段气刨,以减少热量输入,并彻底清除渗碳层,露出金属光泽后方可焊接。

    For the repair of stainless steel, to reduce heat energy and clean completely, gouging should in discontinuous way.

    youdao

  • 通过对13 -5型马氏体不锈钢焊接接头进行等离子弧清根及碳弧气刨清根的比较,证明等离子弧清根对全焊透焊缝实施背面清根是可行的。

    By comparing backgouging of plasma arc with carbon arc to the welded joint of 13-5 martensitic stainless steel, the backgouging of plasma arc is proved feasible for the full penetration weld.

    youdao

  • 通过对13 -5型马氏体不锈钢焊接接头进行等离子弧清根及碳弧气刨清根的比较,证明等离子弧清根对全焊透焊缝实施背面清根是可行的。

    By comparing backgouging of plasma arc with carbon arc to the welded joint of 13-5 martensitic stainless steel, the backgouging of plasma arc is proved feasible for the full penetration weld.

    youdao