在核压力容器钢的中子辐照脆化评价中,断口剪切面积百分比是一个重要的参数。
Percent shear fracture appearance is an important factor to evaluate neutron irradiation embrittlement of nuclear pressure vessel steel.
本文提出了基于支持向量机模型预测钢淬透性的方法,并分析了核函数的选择对支持向量机建模的影响。
In this paper, an SVM-based approach applied to predict steel quenching degree is presented, and the effects of selecting kernel function on SVM modeling are also analyzed.
结果发现,TWIP钢具有典型的延性断裂断口特征,其变形和断裂过程为微孔洞的形核、长大和聚合。
It was found that the fracture of TWIP steel was typical ductile fracture pattern and its deformation and fracture processes were the formation, growth and coalescence of microvoids.