结果表明,大尺寸的非金属夹杂和背帽外缘的点焊是引起泵轴过早断裂的主要原因。
The fracture of the pump shaft is mainly caused by large size non metallic inclusions and point welding between the lock nut and the pump shaft.
注水结束后,扩张区切取含胸背动脉的轴型皮瓣移植在邻近新造皮肤缺损区。
After dilatation, axial pattern skin flap, which contained thoracodorsal artery, was displaced to the new defect skin area nearby.
该类型泵特别适合于低比重介质的工况, 在这种情况下背对背的设计及中间衬套可以产生自然的轴向平衡和附加的轴支撑。
They are particularly suited to low specific gravity applications where the back-to-back design and center bush provide natural axial balance and additional shaft support.
应用推荐