淬火裂纹深而细长,断口平直,破断面。
Quenching crack deep and long, straight fracture, fracture surface without oxide color.
破断面观察结果显示,在室温中,氢气会导致平滑试片在表面形成裂纹,而在凹槽试片中产生劈裂破坏形态。
Fractographic observations showed that hydrogen could induce surface cracks for smooth specimens and a cleavage fracture pattern for notch specimens at RT.
影响井巷稳定性的因素主要有:围岩性质、井巷位置、巷道轴线方向,断面尺寸,破岩方法等。
The factor that affect the well lane stability has primarily: Round the rock kind, well lane position, tunnel stalk line direction, cross section size, break rock method etc.
应用推荐