结果表明:直接淬火工艺的淬火组织为板条马氏体和孪晶马氏体共存,且孪晶马氏体的含量较多。
The results show that the quenching microstructure of direct quenching technology consists of lath and twin martensites, and the amount of the latter is more.
淬火组织中马氏体与残余奥氏体的成分不均匀及磨削用量参数选择不当是导致裂纹出现的主要原因。
Uneven components of quenched martensite and residual austenite structure and improper grinding parameter are attributed to the main causes for cracks.
根据试样任意一点的温度和冷却速度对该点的组织进行预测,实现了T8钢淬火组织的计算机模拟。
According to the temperature and rate of cooling, microstructure forecast is carried out, computer simulation of quenching microstructure of T8 steel is accomplished.