结果表明,经过阻燃处理的木材其氧指数和剩碳率比未处理的木材升高,而热降解反应活化能和分解温度降低。
Experimental data showed that for the treated wood there was an increase in char yield and LOI, and decreases in activation energy and temperature of decomposition.
这种活化形式对于治疗非常重要,因为活化的形式比CPT - 11高1000倍。
This activation is essential to treatment because the activated form is up to 1,000 times more active than CPT-11.
磷酸活化活性炭的孔隙结构能通过调整磷酸浓度、浸渍比和炭活化温度进行控制。
Subsequently, the porosity of activated carbon can be controlled by modification of the concentration of phosphoric acid, impregnation ratio and activation temperature.