结果表明,选择酚醛树脂硫化体系、控制酚醛树脂用量为5 份以及EPDM/PP共混比为50/50,可以得到挤出表面最为光滑的共混物。
The results showed that the extrudate with the most smooth surface was obtained when 5 phr of phenolic resin and 50/50 blending ratio of EPDM/PP were used.
硫化体系采用酚酸树脂2402/氯化亚锡(8/0.5)、加入一定量的增塑剂邻苯二甲酸二辛酯和补强剂高耐磨炭黑,可获得性能较好的共混体。
A blend with better properties could be obtained by adding phenolic resin 2402/tin bichloride (8/0. 5) curative and a certain level of dioctyl phthalate plasticizer and HAF reinforcing agent.