水处理剂、高矿化度高钙镁离子和残留聚合物对AP-P4溶液粘性模量的损失较大;
Water treatment agent, high salinity , high calcium and magnesium ion and produced polymer have largely lost the viscous modulus of the AP-P4 solution.
结果表明,在热湿条件下老化结束后,材料的断裂应力、初始模量和断裂比功的损失率分别大于44%、65%和51%;
The results showed the loss rates of stress, initial modulus and breaking work were more than 44%, 65% and 51% after hydrothermal aging test respectively;