结果表明,锰回收率大于97%,钴总回收率大于95%,镍总回收率大于90%。
The results show that total process recovery is up to 97% for Mn, 95% for Co and 90% for Ni.
同时采用精选补加硫化钠抑制石英,得到了含硅量低于1.0%,品位高于97%,总回收率高于87%的高品级萤石。
By adding sodium sulphide to depress quartz in the cleaning, high grade fluorite concentrate can be gained, whose content of silicon is under 1.0%, grade is over 97% and recovery is higher than 87%.
该工艺浸出率达97%以上,锌总回收率达92 %以上,并可实现铅锌分离。
Using this technology, the leaching yield over 97% and recovery yield of zinc over 92% and separating of lead zinc could be realized.