·2,447,543篇论文数据,部分数据来源于NoteExpress
结果得出:阀体失效的主要原因是阀体本身存在严重的铸造缺陷,铸造疏松严重、孔洞尺寸大乃于形成原始裂纹源;
The results showed that the root reason for valve body failure was seriously casting defect exist and its big and density shrinkage porosity form the original crack;