Uranium and Impurity in U3O8 八氧化三铀中铀和杂质元素成分分析标准物质

双语例句

  • After exposure to carbon monoxide, contents of oxygen in the surface oxides of uranium metal and U3O8 are decreased and O/U ratios decrease 7. 2% , 8.0% respectively.

    一氧化碳气氛中金属表层氧化物八氧化三铀含量减少O/U比值分别下降7.2%和8.0%。

    youdao

  • The use of U3O8 additive can improve the pellet microstructure, but result in decrease of pellet density and increase of open porosity, which contributes strongly to moisture.

    采用U_3O_8添加剂改善芯块微观结构同时使芯块密度下降开口孔隙度增加进而导致吸湿加剧。

    youdao

  • The surface structures of uranium metal and triuranium octaoxide (U3O8) and the influence of carbon monoxide to the surface layers have been studied by X-ray photoelectron spectroscopy (XPS).

    X射线光电子能谱(XPS)分析研究了金属表层八氧化三铀表面结构以及一氧化碳表面结构影响