Hardness can do 61 — 65hrc maturation process is: annealing, softening after casting machining, machining of air cooling after quenching and low temperature stress tempering.
硬度能做到61——65hrc成熟工艺是:铸造后软化退火,便于加工,加工后空冷淬火加低温去应力回火。
According to the tempering temperature and hardness curve, the redistribution of residual stress is associated with the transformation of residual austenite.
由回火温度与硬度变化曲线证实,残余应力重新分布是与残余奥氏体转变相关联。