Through four-point bending test, the effect of curing temperature on flexural properties of PVA-UHTCC has been investigated by means of standard curing at 20°C and water-bath curing at 55℃.
通过四点薄板弯曲试验采用20℃标准养护和55℃水浴加速养护研究了温度对PVA-UHTCC弯曲性能的影响。
参考来源 - 粉煤灰对超高韧性水泥基复合材料弯曲性能的影响试验研究·2,447,543篇论文数据,部分数据来源于NoteExpress
Standard curing periods were respectively 0,2,6,27days, trial age was 28 days.
标准养护的时间分别为0天,2天,6天和27天,试验龄期均为28天。
Standard curing periods were respectively 0, 2, 6, 27days, trial age was 28 days.
标准养护的时间分别为0天,2天,6天和27天,试验龄期均为28天。
The dry shrinkage rate of standard curing concrete sand mortar evidently exceeded the steam curing simples at the same age.
标养水泥砂浆的干缩率明显大于同龄期蒸养水泥砂浆试件。