An overall chromium coating improves the corrosion resistance of the generally used through-hardening rolling bearing steel.
一个总铬涂层提高了耐腐蚀性能的普遍使用,通过硬化滚动轴承钢。
Compared with the strip produced by conventional austenite rolling, the yield strength of the ferrite rolled strip was lower by about 20%, with same elongation and strain hardening exponent.
相对于常规奥氏体轧制,铁素体轧制薄板的屈服强度下降了20%左右,伸长率及应变硬化指数与之相当。
The results show that the effects of work hardening by strain-induced martensite transformation and cast pore defects are the main reasons leading to strip broken of the steels during cold rolling.
结果表明,形变诱发马氏体组织所加剧的加工硬化与冶炼时所产生的气孔缺陷的共同作用是冷轧断带的原因。