And the mechanism of Cu/Al roll cladding was analyzed. In order to satisfy the forming property (bending property), heat treatment of Cu/Al rolling clad sheet should be at a low temperature, especially at 350℃for one hour.
在提高材料成型性能(弯曲性能)的要求下,铜/铝轧制复合板适合选择的低温退火制度,以350℃,1小时以内为宜。