It is concluded that the local tensile stress created during quenching process and the stress concentration due to sharp V-shaped notch are the primary reasons of cracking.
认为,淬火过程中产生的局部拉应力加上尖锐V型槽口引起的应力集中是造成开裂的主要原因。