高温预析出对7055铝合金组织和力学性能的影响 - TNMSC 关键字: 7055铝合金; 固溶; 预析出; 应力腐蚀[gap=804]Key words: 7055 alloys; solution; pre-precipitation; stress corrosion
基于32个网页-相关网页
L10 pre-precipitation phase L10早期沉淀相
pre-precipitation at high temperature 高温预析出
Pre-precipitation treatment at 370℃ incurred pre-precipitates in the grain and GB.
而在370℃预析出处理将导致晶内和晶界同时析出。
参考来源 - 高温预析出对Al·2,447,543篇论文数据,部分数据来源于NoteExpress
The effects of high temperature pre-precipitation on the stress corrosion properties of the heat affected zone were also studied after welding.
并研究了高温析出对焊接热影响区及后处理应力腐蚀性能的影响。