... 冲击磨耗 pounding wear 浇铸性 pourability 浇铸不足(铸疵) poured short ...
基于2个网页-相关网页
-
流动性
- 引用次数:1
As a result the tensile strength of the alloy is 453 MPa and the elongation is 14%. The alloy also has better pourability and has slight thermal cracking tendency.
该合金的流动性较好,热裂倾向小,热处理后抗拉强度可达453MPa,延伸率为14%。
参考来源 - 高强度铸造Al
可浇注性
·2,447,543篇论文数据,部分数据来源于NoteExpress