A blend with better properties could be obtained by adding phenolic resin 2402/tin bichloride (8/0. 5) curative and a certain level of dioctyl phthalate plasticizer and HAF reinforcing agent.
硫化体系采用酚酸树脂2402/氯化亚锡(8/0.5)、加入一定量的增塑剂邻苯二甲酸二辛酯和补强剂高耐磨炭黑,可获得性能较好的共混体。
Dibutyl phthalate is commonly employed as such a plasticizer.
酞酸二丁酯一般用来作为这类增塑剂。
In addition, 25 PHR of cold resistant plasticizer (dibutyl phthalate 10 PHR; dioctyl sebacate 15 PHR) were added into NBR compound to improve th.
另外,在NBR胶料中添加25份耐寒增塑剂(邻苯二甲酸二丁酯10;癸二酸二辛酯15)。
应用推荐