Cobalt ferrite and nickel ferrite with uniform particle sizes in the range of 10-50 nm can be obtained by using nitrates or acetates as raw materials. The optimal temperature and reaction time are 200-220℃and 24-48 hours, respectively.
以硝酸盐或醋酸盐为原料用混合碱法可制得粒度均匀、粒径范围在10-50nm的钴铁氧体、镍铁氧体,其较合适的反应温度为200-220℃,反应时间为24-48小时,所制备的样品具有粒径小、粒度均匀、分散性较好的特点。