Nanoindentation has been widely used to evaluate and test material properties, we utilize the unloading curves of an indentation test to extract the hardness and reduced modulus of the material.
纳米压痕技术广泛用于材料力学性能的评估与测试,利用压痕的加卸载曲线可分析得到材料的硬度和折合模量等力学参数。
In this paper, the mechanical properties of the amorphous ribbon are investigated by nanoindentation, and the obtained results are compared with the measuring results of tensile test.
文章采用纳米压痕测量技术研究其机械性能,并且与拉伸试验测得的结果进行了比较。