compound molten salt method 复合熔盐法
prepared by molten salt method 熔盐法制备
Low-temperature molten salt method 低温熔盐法
molten salt coating method 熔盐包裹法
The CCTO nanorods were successfully prepared by molten salt method. Thediameters of the nanorods are about 50~80nm, and 100~250nm of length.
然后,通过改进熔盐法一步反应合成了CCTO纳米棒,纳米棒直径大约50~80nm,长度达到100~250nm。
参考来源 - 新型类钙钛矿高介电常数氧化物的制备与结构表征·2,447,543篇论文数据,部分数据来源于NoteExpress
应用推荐