The brittle morphologies become much more notable, and appear the inter-and trans-granular fracture mode after sodium corrosion at high temperature for both of W-specimens.
钠腐蚀后,两种钨试样的沿晶脆断特征变得更为显著,为沿晶和穿晶混合型脆性断裂。
The rupture reasons of tube joint weld of the stainless steel pressure meter are analyzed. It is characteristic of stress corrosion cracking and inter granular fracture.
分析了不锈钢压力表管接头焊缝开裂的原因,认为此种开裂具有应力腐蚀开裂、沿晶断裂特征。