inside weld seam 内焊缝
inside weld tiny crack 内焊缝微裂纹
inside corner weld 内角焊接
inside fillet weld 内角焊接
inside weld grinding machine 内焊缝磨削机
inside weld surface treatment 内焊缝表面处理
Hot cracks commonly occurred in inside weld as the forming process of SSAW pipe.
螺旋埋弧焊管在成型过程中容易产生内焊热裂纹。
Inside weld produced cracks are often faced problem by adopting wide coil with small forming Angle to produce small size spiral submerged welded pipe.
采用宽板小成型角生产小口径螺旋缝埋弧焊钢管时,内焊缝产生裂纹是经常遇到的问题。
Through analysis on inside weld forming and welding procedure of SSAW pipe, it pointed out weld crack is easy to appear in brittle temperature zone in welding pool.
通过对螺旋埋弧焊管内焊缝成型和焊接过程的分析,指出焊缝裂纹易产生在焊接熔池脆性温度区。