High quality Fe3O4 octahedral particles of ~500nm were successfully synthesized from iron powders by simple hydrothermal treatment with 10 M NaOH at 180°C.2.
1、通过在水热条件下浓碱处理铁粉,成功的制备了直径~500nm的均匀的高质量的四氧化三铁八面体粒子。
参考来源 - 铁氧化物纳米材料的形貌可控合成及性质研究Preparation and characterize of Fe3O4 nanometer drugThe Fe_3O_4 gelatin composite nanoparticles and Fe_3O_4 nanometer drugs were synthesized by the coacervated method using isopropanol as coacervation reagent. And we explored the best ratio of the preparation of Fe3O4 gelatin composite nanoparticles.
4.强磁性四氧化三铁明胶纳米药物的制备与表征采用单凝聚法制备了Fe_3O_4磁性明胶纳米药物载体,探索了制备磁性纳米微球的最佳配比。