Wax precision casting is adopted for the shaft sleeve, increasing material utilization ratio by 77% and realizing "less cutting and no cutting".
铸造工艺采用石蜡精铸成型,使材料利用率提高77%,达到少切削、不切削目的;
All of the casting dimension precision, surface roughness and material control have reached national standard.
铸件尺寸精度,表面精糙度及材质控制均达到国家标准要求。
应用推荐