Through cyclic voltammetric analysis,oxygen evolution potential at DSA anode prepared on 700℃is highest.
通过循环伏安分析表明700℃表层电极的析氧电位最高。
参考来源 - 稳定阳极的制备、表征及其与活性炭联用的三维电解法在废水处理中的应用·2,447,543篇论文数据,部分数据来源于NoteExpress
These superior performances can be attributed to the higher reaction activity, lower electrochemical impedance and higher oxygen evolution potential for the nanostructured nickel hydroxide electrodes.
添加有纳米结构粉末的镍电极具有更高的反应活性及更小的电化学反应阻抗,充电时氧气析出电位也比较高,因而表现出优良的电化学性能。
The volume of oxygen evolution on lead was smaller than that on lead-bismuth alloy at the same anodic potential.
氧气收集实验表明,相同电位下,纯铅电极上收集到的氧气的体积稍小于铅铋合金电极;
The research progress in lowering the hydrogen generating energy consumption of alkaline water electrolysis by decrea-(sing) the anodic over potential for oxygen evolution was reviewed.
综述了通过降低阳极析氧过电位来减少碱性水电解制氢能耗的研究进展。