defect in the weld 焊接缺陷
Since there are weld defects in welds, using traditional strength theory based on no defect and no crack to design, crane's security in rating load can't be insured.
由于在焊缝部位存在焊接缺陷,采用传统的建立在构件无缺陷、无裂纹基础上的强度理论进行设计计算时,往往不能确保起重机在额定载荷下使用的安全性。
The ultrasonic phased array system for monitoring the expanding of weld defect in steel bridge was researched.
研制了针对钢结构桥梁焊缝缺陷扩展的超声相控阵监测系统。
The research focuses on the defect equivalent analytical methods in building steel structure butt weld fusion and the effects of non-crack-type defects on the normal use of butt weld fusion.
本课题研究了建筑钢结构熔透对接焊缝中缺陷当量的分析方法和非裂纹类缺陷对焊缝正常使用的影响。