... intermediate temperature creep 中温蠕变 room temperature creep 室温蠕变 high temperature tensile creep 高温拉伸蠕变 ...
基于8个网页-相关网页
K 46合金的高温拉伸蠕变曲线表现出非常长的稳态蠕变阶段,而较高的蠕变塑性来自于加速蠕变阶段。
It is found that the creep curves of alloy K46 consist mainly of a longer steady-state creep stage and an accelerated creep stage, which occupies the most creep strain.
研究了一种无钴镍基铸造 高温合金K46的 高温拉伸、蠕变和持久性能,并与K412合金进行了比较。
The tensile, creep and stress-rupture properties at high temperature of a cast nickel-base superalloy K46 without cobalt, as comparison with superalloy K412, were investigated.