分析大直径高强度镀锌钢丝拉拔困难的主要原因在于锌-铁合金层较厚、钢丝中碳含量和锰含量较高。
It is indicated by analysis that the main causes of difficulty of drawing high strength thick galvanized steel wire are thicker ZnFe alloy coat and higher carbon and manganese contents.
通过采用小压缩率多道次拉拔工艺,减少锌-铁合金的厚度,积极采用人工时效工艺等解决了拉拔困难的问题。
The drawing difficulty is settled by adopting small draught and multi-pass drawing process, reducing the thickness of Zn-Fe alloy and using artificial aging process actively.
采用正交试验法对锌-铁合金镀层三价铬黑色钝化工艺进行优化,并研究了工艺参数对钝化膜外观和耐蚀性等影响。
The bath compositions of trivalent chrome black passivation for zinc-iron alloy coating were optimized by orthogonal test method.