... internal pressure stress 内压应力 internal rail stress 钢轨内部应力 internal-stress-induced plastic flow 内应力引起的塑性流动 ...
基于8个网页-相关网页
钢轨残余应力是钢轨内部的固有应力。 它影响钢轨的使用寿命。
The residual stress is the inherent stress in rails, it affects the life of rails.
youdao
自然环境条件下的温度变化会在钢轨内部产生拉伸应力,影响无缝线路轨道的稳定性。
The variability of weather and climate is a cause of considerable stress to CWR track which has influence on the stability of rail.