此炉子已经成功地用于铁精矿粉还原焙烧,所得到的海绵铁产品的金属化率大于92 %,全铁约90 %。
Continuous car type furnace was used in iron ore reduction successfully. The contents of with rotary hearth furnace are as more than 92% metallization and about 90% total iron.
重点分析了在焙烧过程中,棒形产品和瓷套产品黄芯缺陷的形成过程,认为该缺陷是坯件在焙烧过程中还原不足造成的。
The formation process of tawny core defect in porcelain bydy of insulator at firing were be analysis in detail. The author atributes it to the body was not deoxidized safficiently at firing.