通过对45钢两种试样状态及冶炼、轧制工艺的分析,找出了白点是导致45钢断面收缩率不合的根本原因,钢中氢含量高是内因,轧后冷速过快是外因。
By analyzing the states of two samples and smelting and rolling process, it was found out that the essential reason resulting in area reduction disqualification of Steel 45 was flake.