... 体积电阻率(Volume resistivity) 老化后断裂伸长率(Elongation after aging) ※化学性能(Chemical): ...
基于826个网页-相关网页
老化后断裂伸长率 Elongation after aging ; Ultimate elongation After aging ; Elongation at break after aging 老化后的断裂伸长率 Elongation after Aging 纺织品 卷装纱 单根纱线断裂强力和断裂伸长率的...
基于80个网页-相关网页
老化后断裂伸长率 ( Elongation at break after aging ): ≥% 180 断裂伸长率最大变化率(Max change of elongation at break): ≤% ±20
基于28个网页-相关网页
老化后的断裂伸长率 Elongation after Aging
对试样进行了硬度、拉伸强度、断裂伸长率、热老化等性能试验;对老化后的试样表面进行了SEM表征。
Hardness, tensile strength, breaking elongation ratio and aging property of samples were tested and surface of sample after aging was represented by SEM.
添加黑液干粉的复合材料,在热氧老化后拉伸强度和邵尔A型硬度增加,断裂伸长率稍有下降。
In general, the tensile strength and Shore A hardness of PVC/CPE/black liquor powder composites were increased while the elongation at break was slightly decreased after thermo-oxidative aged.