在此工艺条件下,制得的无水氯化钪熔盐中钪的水解率为2.3%。
Under the optimum technology condition, we can get the anhydrous scandium chloride molten salt whose hydrolysis rate is2.3%.
本发明使用的电解质为氯化钙熔盐体系,可 在其中掺入氯化钠、氯化锂或它们的混合物。
The electrolyte used in the invention is a calcium chloride fused salt system, into which sodium chloride, lithium chloride or admixture of the sodium chloride and the lithium chloride can be admixed.