  limiting drawing ratio

...成形性能;极限拉深比[gap=1267]Key words: 5182 aluminum alloy; warm deep drawing; forming property; limiting drawing ratio...

基于22个网页-相关网页

  limit drawing ratio

...极限拉深比;温热成形 [gap=684]Keywords : high strength aluminum alloy;non-isothermal warm forming;limit drawing ratio;warm forming or hot formingzz')" href="#"> ..

基于16个网页-相关网页

  • limiting drawing ratio - 引用次数:2

    The results show that, under the condition of forming temperature of 225℃and deep drawing velocity of 1mm/s, limiting drawing ratio 3.0 can be obtained.

    在高温下,拉深速度增加,极限拉深比减小,并在225℃,拉深速度为1mm/s时,成功的制成了拉深比3.0的平底筒形件和球底筒形件。

    参考来源 - AZ31镁合金筒形件热拉深成形
    limit drawing ratio - 引用次数:2

    参考来源 - C2680黄铜箔微圆筒拉深工艺研究

·2,447,543篇论文数据,部分数据来源于NoteExpress

双语例句

  • 文中给出锥形件一次成形极限拉深图线数表可供生产实用。

    The curves and data of limit drawing ratio, which can be applied in production, are given.

    youdao

  • 采用可以明显提高板材的冲压性能极限拉深达到5.0。

    Using variable blank holder force can remarkably improve the forming performance, and the limiting drawing ratio would reach 5.0.

    youdao

  • 研究变形温度、变形速度铸轧az31镁合金极限拉深(ldr)组织影响。

    The effect of deformation temperature and deformation speed on the limit drawing ratio (LDR) and microstructure of the roll-casting AZ31 magnesium alloy sheet.