在应变疲劳曲线上,弹性线和塑性线的交点随弹簧钢回火后硬度的升高而向低循环寿命移动;
The point of intersection of elastic line and plastic line moves toward the low cycle life with the hardness of the spring steel raised after tempering from the strain fatigue curve.
研究结果表明,弹塑性有限元分析法预测的寿命偏低,由残余应力可以较准确地确定最大应力应变循环。
The result shows that predicting life by elasticity-plasticity finite element analysis is low and the maximal stress-strain cycle can be calculated accurately by the residual stress method.
喷丸过程和随后的接触疲劳滚压过程同属在赫兹应力作用下的循环弹塑性应变过程。
Both shot peening and contact rolling belong to the cyclic elastic-plastic deformation process under the action of Hertz stress.