得到了镍基喷焊层元素熔入量对奥氏体焊缝显微组织及裂纹敏感性的影响规律。
The influencing rules of the content of alloy elements in nickel-base spraying layer on the microstructure of austenite weld and the crack sensitivity were found.
平衡铁素体和奥氏体两相组织在焊缝金属和热影响区中的比例,保证焊接接头的性能,是双相不锈钢焊接的基本要求。
The basic requirement of welding the steel 2205 is that the weld metal and heat-affected zone obtain a favorable phase balance and retain the performance as the base metal after welding.
研究结果表明:在不预热条件下,用KD286焊补钢轨,焊缝组织为柱状奥氏体组织,熔合区和过热区不可避免地产生脆硬的马氏体组织。
The results show that:under the no preheating condition, the microstructure of weld metal is columnar austenitic, and brittle martensite exists in the fusion zone and over-heated zone unavoidably.