Between 2%~10% pre-strain, the shape recovery ratio of SMA decreases continuously, and the shape recovery stain ε_rincreases first and then decreases with the rising of pre-strain.
在2%~10%范围内,随着预应变量的提高,试样形状记忆回复率不断下降,可回复应变量呈先升高后降低的趋势。