其中以粉煤灰50%、硅灰10%取代普通硅酸盐水泥的试验组,无论是试验室标准养护或是加速老化试验都表现出最优的耐久性。
Among which the experiment group using 50% fly ash, 10% silica fume instead of ordinary Portland cement shows rather better durability either in standard curing or the accelerated aging experiment.
养护工艺通常分为自然养护、太阳能养护、蒸汽养护及加速硬化等。
The curing technologies are usually classified as natural curing, solar energy curing, steam vapor curing, accelerated hardening curing, etc.