以丁醇钛、乙醇锆、醋酸铅为原料,采用溶胶-凝胶新工艺,成功地制备出锆钛酸铅陶瓷材料。
Lead Zirconate Titanate ceramic material has been prepared by sol-gel method with Titanium butoxide, Zirconium alkoxide and anhydrous lead acetate.
用醋酸锂和乙醇钽作为起始反应物,通过溶胶凝胶工艺生成了对红外敏感的钽酸锂薄膜,并详细讨论了基于钽酸锂薄膜的红外探测器件制备工艺。
The LiTaO3 thin film was chosen as infrared sensing film and prepared by a sol-gel process using lithium acetate and tantalum ethoxide as starting materials.