通过宏观及微观检测,分析了6061铝合金管及A7003铝合金薄壁管经TIG(氩弧)焊后的焊接区开裂的原因。
After visual inspection and metallographic test, analysis and discuss the welding zone cracking reasons for 6061 and A7003 aluminum alloy thin-walled tube after TIG (argon shielded arc) welding.
探讨氦-氩混合气体保护下tig焊接az31镁合金板的可焊性,对其焊接工艺参数进行确定。
The weldability of AZ31 magnesium plate by He-Ar mixed gas tig welding was investigated. The welding process parameters for AZ31 plate with a 3 mm thickness were optimized.