solid concentration cells 浓差电池
gas concentration cells 气体浓差电池
Severe corrosion, leading to pitting, is often caused by concentration cells, particularly where differences in dissolved-oxygen concentration occur.
特别在溶解氧浓度有差别的场合,浓差电池常引起严重腐蚀、导致孔蚀。
They allow a certain amount of salt to enter their cells, bringing the salt content of the water within the plant, to a slightly higher concentration than that of the surrounding seawater.
它们允许一定量的盐分进入它们的细胞,将水中的盐分带进植物体内,并把其体内的盐含量提高到比周围海水稍高的浓度。
The viability of rat glomerular endothelial cells was inhibited by ioversol in a concentration and time dependent manner.
非离子型低渗造影剂碘佛醇能显著降低大鼠肾小球内皮细胞存活率,并呈剂量和时间依赖性。