摘要: 高温合金铸造(casting superalloy)使用精密铸造进行成型的工艺,是高温合金材料制备工艺之一。铸造高温合金在航空、航天和能源领域得到愈来愈广泛的应用。
基于16个网页-相关网页
sx casting superalloy 单晶铸造高温合金
Casting Superalloy M17 铸造高温合金M
aeroengine superalloy casting 航天发动机高温合金铸件
The ingots of cast superalloy K4169 was refined with the addition of a trace of intermetallic compounds to the melt under conventional casting condition.
采用一种新型中间合金复合细化剂,在常规生产工艺条件下对高温合金K4169铸件进行了晶粒细化。
In this paper the effects of pouring temperature, mold temperature, inoculants, and section size on the microstructure and mechanical properties of casting nickel-base superalloy K24 were studied.
本文研究了浇铸温度、铸型温度、孕育剂和截面尺寸对K 24镍基铸造高温合金的组织和性能的影响。
This paper introduces the casting precipitation properties, their effects on the alloy microstructure and the methods to eliminate the precipitation of the Low-expansion superalloy GH909. and GH907.
本文研究了低膨胀高温合金GH907、GH909铸态组织中偏析的性质,偏析对合金组织的影响,以及消除偏析的方法。