casting fine grain 细晶铸造
fine-grain casting 细晶铸造
fine grain casting 细晶铸造
fine grain casting process 细晶铸造
casting fine grain integral turbine 细晶铸造整体涡轮
Improper forging process will also appear large grain or uneven, hardening crack phenomenon, forging cost is higher than the casting flange.
锻造工艺不当也会出现晶粒大或不均,硬化裂纹现象,锻造成本高于铸造法兰。
The casting is usually a fine grain casting with a very fine-grained outer diameter, which is resistant to atmospheric corrosion, a typical situation with pipes.
这种铸件通常为外径处晶粒非常细小的细晶粒铸件,能耐大气腐蚀,典型的情况是管子。
The common defects of the housing casting include cracks, sand drop, slag inclusion, shrinkage porosity and rough grain, etc.
机架的常见缺陷有裂纹、掉砂、夹渣、缩孔缩松和晶粒粗大等。