If the set collar end hardness is lower than HRC40, should first on the end surface again a built-up welding hard alloy, after the polish repackaging.
如果固定环端面硬度低于HRC40,则应先在端面上重新堆焊一层硬质合金,经磨光后再装配。
The results show that the wear resistance of built up welding surface of Zn based al alloys are better than that of matrix under the same conditions.
结果表明,在相同条件下,锌铝合金堆焊层的耐磨性高于同种材料母材的耐磨性。
A method to improve the tooth shape of mill roller and adopt the built - up-welding with tungsten carbide on the curved surface of tooth apex has been introduced.
提出了一种改进榨辊齿形并在齿顶弧面上堆焊碳化钨的方法及其加工工艺。
应用推荐