锻造温度,锻造温度控制在820~850℃,当然,如果内在冶金质量不错,锻坯表面质量不错的话,也可在780℃左右轻锻、修光、精整等等。
碳钢正确的锻造温度范围应不包括工业纯铁。
So the correct carbon steel forging temperature range does not include industrial pure iron.
重要的是较低的锻造温度和热处理固溶温度比较高的好得多。
It is important to control the forging temperature and solution treatment temperature lower rather than higher.
研究了不同等温锻造温度对2b70铝合金显微组织与力学性能的影响。
The effect of isothermal forging temperature on microstructure and mechanical properties of2B70 aluminum alloy was studied.