... fracture aperture 裂缝开度 fracture appearance transition temperature 裂纹扩展转变温度 fracture azimuth 裂缝方位 ...
基于44个网页-相关网页
管道裂纹的扩展速度主要取决于管道钢的转变温度FATT。FATT可由落锤撕裂试验测定。
The crack propagation rate of pipes is mainly dependent on FATT of Steels of pipes (fracture appearance transition temperature). And FATT can be measured by drop weighted tear tests.
介绍了管道裂纹的扩展速度主要取决于管道钢的转变温度FATT, FATT可由落锤撕裂试验测定。
The crack propagation rate of pipes was mainly dependent on FATT "of pipeline steel, and FATI" can be measured by drop weight tear test.